Home / Shop / SuperHDT 3D Printer Resin, Highest Heat Deflection Temperature 464°F, Made in Korea by 3DMaterials (1000g, Amber)
  • SuperHDT 3D Printer Resin, Highest Heat Deflection Temperature 464°F, Made in Korea by 3DMaterials (1000g, Amber) - Poueer
  • SuperHDT 3D Printer Resin, Highest Heat Deflection Temperature 464°F, Made in Korea by 3DMaterials (1000g, Amber) - Poueer
  • SuperHDT 3D Printer Resin, Highest Heat Deflection Temperature 464°F, Made in Korea by 3DMaterials (1000g, Amber) - Poueer
  • SuperHDT 3D Printer Resin, Highest Heat Deflection Temperature 464°F, Made in Korea by 3DMaterials (1000g, Amber) - Poueer
  • SuperHDT 3D Printer Resin, Highest Heat Deflection Temperature 464°F, Made in Korea by 3DMaterials (1000g, Amber) - Poueer
  • SuperHDT 3D Printer Resin, Highest Heat Deflection Temperature 464°F, Made in Korea by 3DMaterials (1000g, Amber) - Poueer
  • SuperHDT 3D Printer Resin, Highest Heat Deflection Temperature 464°F, Made in Korea by 3DMaterials (1000g, Amber) - Poueer
  • SuperHDT 3D Printer Resin, Highest Heat Deflection Temperature 464°F, Made in Korea by 3DMaterials (1000g, Amber) - Poueer

SuperHDT 3D Printer Resin, Highest Heat Deflection Temperature 464°F, Made in Korea by 3DMaterials (1000g, Amber)


  • [Heat Deflection Temperature 464 °F] Highest heat deflection temperature of 464 °F in the world.
  • [Increase HDT by adding SuperHDT] Adding SuperHDT to standard resins increase the HDT of print substantially.
  • [User Guide #1 Remelting Resin] Please check the color before use, warm the bottle at 140°F for an hour or 120°F for couple of hours.
  • [User Guide #2 Post-curing] Post-curing by 20mW/cm2 395nm ~ 405nm LED light for 10 minutes, and heating up the print in 176°F oven for one hour.
  • [ISO 10993-5] Properly cleaned and fully post cured SuperHDT prints pass ISO 10993-5 test.
Quantity
ADD TO CART
BUY IT NOW
  • Detail
    High HDT 3D printer resin, rigid ceramic, flame retardant (UL 94), for electric engineering.
    • The settings chart is available at the end of this page, or you can download it from the Amazon document list using QR code on the label of bottle.

    • Use alcohol to remove excess resin from the surface and dry the prints completely. Post-cure them using any brand’s curing machine for 20 minutes in air. One tip is the underwater (without oxygen) curing for another 10 minutes gives better result.

    Customer Reviews